Jump to content

Search the Community

Showing results for tags 'flute'.

  • Search By Tags

    Type tags separated by commas.
  • Search By Author

Content Type


Forums

  • Ceramic Arts Daily Forums
    • Forum FAQ & Terms of Use
    • Studio Operations and Making Work
    • Clay and Glaze Chemistry
    • Equipment Use and Repair
    • Business, Marketing, and Accounting
    • Educational Approaches and Resources
    • Aesthetic Approaches and Philosophy
    • Int'l Ceramic Artists Network (ICAN) Operations and Benefits
    • Ceramic Events of Interest
    • Community Marketplace – Buy/Sell/Trade/Free

Find results in...

Find results that contain...


Date Created

  • Start

    End


Last Updated

  • Start

    End


Filter by number of...

Joined

  • Start

    End


Group


AIM


MSN


Website URL


ICQ


Yahoo


Jabber


Skype


Location


Interests

Found 2 results

  1. From the album: Ocarinas, Flutes, & Aerophones

    Fully functional ocarina/flue that plays one octave. Handbuilt stoneware, approximately 12" tall, with red iron oxide stain, Amoco Velvet underglaze, and clear glaze fired to cone 10 reduction.

    © Copyright 2016 - Paul M. Chenoweth - Nashville, TN USA - All rights reserved.

  2. From the album: Ocarinas, Flutes, & Aerophones

    These three instruments represent the experimentation with building, glazing, and firing ocarinas (flutes) over the period of 2013, 2014, and 2015. The shadowbox idea is the direction I plan to take for displays, although the lighting may need some help by a minor adjustment in the box depth. Friends here on the CAC Forum might recognize the "Witch is Dead" themed piece in the middle as a spin-off of a Community Challenge project.