Hello! I was wondering if anyone could make a suggestion since last night I did a bisque fire at 04 cone. When I opened the kiln today the cone was completely straight, however it seemed the kiln did a full fire as I set the timer to 7 hours total and have never gone over that time span. I've used this method many times and have always gotten normal 90 degree bent cones so I was so taken back when the cone appeared as if no firing was done ? Could I of just gotten a defective cone ? I've used about 10 from the same pack with no issues. It's the strangest thing... I've never us
- 8 replies
-
- kilnsitter
- kilnsitter; cone
-
(and 1 more)
Tagged with:
-
I somehow managed to put on a 15 hour HOLD instead of a 15 hour delay on a bisque meant for cone 04. Any ideas as to what cone that actually hit? I’m so scared to open the kiln. Still cooling. It held around 1900° for 15 hours. Clay is cone 6.