Jump to content

Search the Community

Showing results for tags 'chopstick jar'.

  • Search By Tags

    Type tags separated by commas.
  • Search By Author

Content Type


Forums

  • Ceramic Arts Daily Forums
    • Forum FAQ & Terms of Use
    • Studio Operations and Making Work
    • Clay and Glaze Chemistry
    • Mold Making and Slip Casting
    • Equipment Use and Repair
    • Business, Marketing, and Accounting
    • Educational Approaches and Resources
    • Aesthetic Approaches and Philosophy
    • Int'l Ceramic Artists Network (ICAN) Operations and Benefits
    • Ceramic Events of Interest
    • Community Marketplace – Buy/Sell/Trade/Free
    • Job and Career Opportunities

Find results in...

Find results that contain...


Date Created

  • Start

    End


Last Updated

  • Start

    End


Filter by number of...

Joined

  • Start

    End


Group


AIM


MSN


Website URL


ICQ


Yahoo


Jabber


Skype


Location


Interests

Found 2 results

  1. From the album: Pottery 2016

    White stoneware, thrown on the wheel as a "chopstick" jar and then altered into a teapot. I added the little hand-shaped flower knob. Fired at ^6 in an electric kiln. Laguna's Dynasty Red and Peach Blush, Duncan Concepts Bright Kiwi as the underglazed leaves and stems.

    © Giselle No. 5 Ceramics 2016, all rights reserved

  2. From the album: Wheel Thrown Work, 2015