Hi All, I am trying out barrel firing whilst in lockdown as I do not have access to a kiln. I'm having some problems. The first firing I used the following 60cm pit dug 3-4 inches on fine sawdust pots (some wrapped in foil, some not) Salt Seaweed Red Iron Oxide More sawdust Kindling, then smaller logs up to larger logs Paper to get the fire going. The fire burned for about 2 hours and I think put a lid on and sealed the edges. Next moring it was still quite hot when I took the lid off, so i left it to cool a while. The pots we