Jump to content

Search the Community

Showing results for tags 'White earthenware'.

  • Search By Tags

    Type tags separated by commas.
  • Search By Author

Content Type


Forums

  • Ceramic Arts Daily Forums
    • Forum FAQ & Terms of Use
    • Studio Operations and Making Work
    • Clay and Glaze Chemistry
    • Mold Making and Slip Casting
    • Equipment Use and Repair
    • Business, Marketing, and Accounting
    • Educational Approaches and Resources
    • Aesthetic Approaches and Philosophy
    • Int'l Ceramic Artists Network (ICAN) Operations and Benefits
    • Ceramic Events of Interest
    • Community Marketplace – Buy/Sell/Trade/Free
    • Job and Career Opportunities

Find results in...

Find results that contain...


Date Created

  • Start

    End


Last Updated

  • Start

    End


Filter by number of...

Joined

  • Start

    End


Group


AIM


MSN


Website URL


ICQ


Yahoo


Jabber


Skype


Location


Interests

Found 9 results

  1. From the album: Winter 2016

    Thrown white earthenware, linear additions, Holes carved then dots added. Wash of copper oxide and cobalt carbonate airbrushed when bone dry. Bisqued to 1000oC. Transparent glaze poured over, fired to 1100oC.
  2. From the album: Winter 2016

    Thrown white earthenware, linear additions, Holes carved then dots added. Wash of copper oxide and cobalt carbonate airbrushed when bone dry. Bisqued to 1000oC. Transparent glaze poured over, fired to 1100oC.
  3. From the album: Winter 2016

    Thrown white earthenware, cut and altered. Slabs textured and added. Copper oxide and cobalt carbonate washes when bone dry. Bisqued to 1000oC. Transparent glaze poured over, fired to 1100oC.
  4. From the album: Winter 2016

    Thrown white earthenware, cut and altered. Slabs textured and added. Copper oxide and cobalt carbonate washes when bone dry. Bisqued to 1000oC. Transparent glaze poured over, fired to 1100oC.
  5. From the album: Winter 2016

    Thrown white earthenware, cut and altered. Slabs textured and added. Copper oxide and cobalt carbonate washes when bone dry. Bisqued to 1000oC. Transparent glaze poured over, fired to 1100oC.
  6. From the album: 2016

    Experimenting with bought tissue transfers and stencils as resist. Thrown white earthenware. Dipped in transparent glaze & fired to 1100oC in an electric kiln.
  7. From the album: 2016

    After reading CAD article about making your own transfers, I tried this using a rubber stamp with stain & frit 50:50 mix. Stamped on to tissue paper, applied to leather hard clay. Bisqued to 1000oC. Dipped in transparent glaze & fired to 1100oC in an electric kiln.
  8. From the album: 2016

    Made for a friend's 50th birthday. Various 'significant' words & phrases stamped inside and out with different letter styles, highlighted with oxide washes before bisque firing. Dipped in transparent glaze & fired to 1100oC in an electric kiln.
  9. From the album: 2016

    Small bowl with pinched floral additions. Stains added to transparent glaze painted on flowers. Whole piece dipped in transparent glaze. Fired to 1100oC in electric kiln.
×
×