Slab rolled, fitted into wooden templates I made. Brushed on 3 coats of Mayco cottontail. Fired ^6. Stenciled symbols. Sprigs painted with Mayco SC. Stamped letters.© 2015
- 2 comments
-
- Veganware
- Vegan pottery
-
(and 5 more)
Tagged with:
-
From the album: Veganware
Slab rolled, fitted into wooden templates I made. Brushed on 2 coats Amaco Iron celadon. Fired ^6. Stenciled symbols. Sprigs painted with Mayco SC. Stamped letters.© 2015
- 2 comments
-
- Vegan pottery
- Vegan pottery
- (and 6 more)
-
From the album: Veganware
Slab rolled, fitted into wooden templates I made. Brushed on 2 coats Amaco Wasabi and Lavender celadon. Fired ^6. Stenciled symbols. Sprigs painted with Mayco SC. Stamped letters.© 2015
-