From the album: Custom Mugs and Commission Concepts
These two mugs are a hybrid combination of hand-built and wheel-thrown construction. The rim is the only wheel-thrown piece and is included only because I have never been quite satisfied with my efforts to hand-build rims on mugs. Unique to the stamped-on, tennis net theme are the athletic shoe & tennis ball finials to the pulled handle. The mugs are 14oz-16-oz capacity stoneware, fired Cone 10 reduction. Interior glaze is Woo's Blue. Exterior is clear, sprayed on in two light coats.© Copyright 2017 - Paul M. Chenoweth, Nashville, TN USA - All rights reserved.
- 4 comments
-
From the album: Custom Mugs and Commission Concepts
This is a 12oz-14oz. stoneware mug with a piano/keyboard theme. The rim is wheel thrown and re-assembled into a hand-built, slab-constructed base that has been stamped and stretched/altered. Handle is pulled and attached after the rim is in-place and black keys have been cut from a slab and attached/scored & slipped. Interior and rim is glazed with Woo's Blue. Exterior parts are brushed-on Amaco Velvet underglaze sprayed with a couple of light coats of clear. Mug is fired to Cone 10 reduction.© Copyright 2017 - Paul M. Chenoweth, Nashville, TN USA - All rights reserved.
-
- stoneware
- hybrid wheel-thrown & slab
- (and 4 more)
-
From the album: Custom Mugs and Commission Concepts
These two mugs are a hybrid combination of hand-built and wheel-thrown construction. The rim is the only wheel-thrown piece and is included only because I have never been quite satisfied with my efforts to hand-build rims on mugs. Unique to the stamped-on, tennis net theme are the athletic shoe & tennis ball finials to the pulled handle. The mugs are 14oz-16-oz capacity stoneware, fired Cone 10 reduction. Interior glaze is Woo's Blue. Exterior is clear, sprayed on in two light coats.© Copyright 2017 - Paul M. Chenoweth, Nashville, TN USA - All rights reserved.
-
Hi I'm wondering if anybody has a recipe for a cone 10 reduction copper red glaze (I'm talking oxblood or peach bloom, NOT flambé) that flashes electric blue? I hear that if you use a feldspar based glaze and use a feldspar that is high in potassium and low in sodium (usually its the other way around) that the glaze will tend to have these blue flashes more. If you know a good recipe and have tried it yourself what cone does it work best around? I know that these glazes don't do best at cone 10 but rather around 8-9, but I still wanna hear your experience. Also, I like to do a quick oxidation at the end of my firing in order to make the copper reds less muddy and dark. If you've had good results, how long do you do this oxidation for? Thanks, Hunter
- 2 replies
-
- copper red
- cone 10 reduction
- (and 7 more)
-
Please Help! I have been firing work in a cone ^10 reduction kiln and having problems with my satin black glaze, (see recipe below), coming out with a heavy 'orange peel' texture. Usually it happens on the inside of lidded items--while the outside is a beautiful smooth and metallic satin black. Recently it happened on the inside of a bunch of mugs-usual since it's not a closed form. And at times there is a 'flash' of the 'orange peel' texture on the outside of pieces. Also seems to be happening more often. See attached photo. I should mention that we are firing in a Larson fiber kiln which tends to heat up & cool down quickly. It tends to fire hot-sometime closer to ^11. We usually go into reduction either at ^08 or ^013 depending on the other glazes in the firing. We also often do a 20-30 minute soak at the end-not sure this does anything at all. Does anyone have experience with this or advice? I would love to get rid of the problem entirely but would be happy if it just went back to happening on the inside of lidded pieces. Some of the clay bodies used: B-mix, Black Mountain, Paper Clay Ivory. Have discussed at length with other studio members and thinking it may be the kiln is cooling too fast. Does anyone know a cooling phase for a firing program for an issue such as this? Any thought, ideas, solutions welcome!!! Satin Black Glaze recipe: custer feldspar 1500 Kona F-4 spar 1500 whiting 150 dolomite 1125 silica 1500 ball clay 750 talc 975 bentonite 150 cobalt carb 225 red iron oxide 225 manganese dioxide 150 chrome oxide 150 Many thanks for any help! Len
-
- satin black
- glaze problem
-
(and 3 more)