Jump to content

Search the Community

Showing results for tags 'Charcoal'.

  • Search By Tags

    Type tags separated by commas.
  • Search By Author

Content Type


Forums

  • Ceramic Arts Daily Forums
    • Forum FAQ & Terms of Use
    • Studio Operations and Making Work
    • Clay and Glaze Chemistry
    • Mold Making and Slip Casting
    • Equipment Use and Repair
    • Business, Marketing, and Accounting
    • Educational Approaches and Resources
    • Aesthetic Approaches and Philosophy
    • Int'l Ceramic Artists Network (ICAN) Operations and Benefits
    • Ceramic Events of Interest
    • Community Marketplace – Buy/Sell/Trade/Free
    • Job and Career Opportunities

Find results in...

Find results that contain...


Date Created

  • Start

    End


Last Updated

  • Start

    End


Filter by number of...

Joined

  • Start

    End


Group


AIM


MSN


Website URL


ICQ


Yahoo


Jabber


Skype


Location


Interests

Found 3 results

  1. From the album: Images For Misc. Posts

    Hardwood charcoal is introduced on top of the wares on the last step of Fushigigama once the stoking is complete...at about cone 12-13. Then the kiln is sealed up and the burning charcoal causes reduction cooling effects. The charcoal tends to pop and sizzle into sparks....which you see in this clip.
  2. From the album: Images For Misc. Posts

    The last step of Fushigigama has ports to introduce hardwood charcoal (not charcoal briquettes!) directly onto the load of ware. This is done at the peak of the firing just after ceasing stoking wood and just before sealing up the kiln. Here you can see the general process.
  3. From the album: Kilns designed/constructed by John Baymore

    A single chamber wood fired kiln that was built in Japan at a workshop which I led there in 2006. It is designed to be used for the youhen charcoal finishing process, and you can see the charcoal ports in the wall in the front. It shares a large chimney with a large 5 chamber noborigama (seen behind it). It is fired on a 3 day cycle to 1250 C and then all the ware is buried in wood charcoal for the cooling cycle. This process is heavily used in Bizen. The dubbed this kiln the "Johngama" ( ジョン窯 ) .

    © 2006 John Baymore -all rights reserved

×
×