From the album: John Baymore's Clay Work
Ido-style Chawan. Wood fired and electric fired. Granite bearing stoneware body. American Shino glaze on exterior (with finger wipes), semi-matte feldspathic glaze on interior. Gold luster on interior. Exhibited In "Chawan for Chanoyu" solo exhibition held in conjunction with the 2015 Providence NCECA conference.© 2015 John Baymore -all rights reserved
- 4 comments
-
- Chawan
- John Baymore
-
(and 7 more)
Tagged with:
-
Youhen Mizusashi (water jar for Japanese Tea Ceremony)
Guest posted a gallery image in Browse Member Galleries
From the album: John Baymore's Clay Work
Thrown; yakishime; youhen charcoal finish; noborigama woodfired at Kanayamayaki, Goshogawara-shi, Aomori-ken, Japan; Orton cone 14. Private collection in Japan.© John Baymore 2013 - all rights reserved
- 2 comments
-
- Youhen
- Noborigama
-
(and 6 more)
Tagged with:
-
American Shino Glaze Mizusashi (water jar for Japanese Tea Ceremony)
Guest posted a gallery image in Browse Member Galleries
From the album: John Baymore's Clay Work
Thrown; noborigama woodfired; Orton cone 12; American Shino glaze. In the Tsinghua University collection in Beijing.© John Baymore 2011 - all rights reserved
- 3 comments
-
- American shino
- Shino
-
(and 7 more)