From the album: 2016
Experimenting with bought tissue transfers and stencils as resist. Thrown white earthenware. Dipped in transparent glaze & fired to 1100oC in an electric kiln.- 3 comments
-
- Tissue transfers
- stencil
-
(and 2 more)
Tagged with:
-
White earthenware bowl with floral additions
Celia UK posted a gallery image in Browse Member Galleries
From the album: 2016
Small bowl with pinched floral additions. Stains added to transparent glaze painted on flowers. Whole piece dipped in transparent glaze. Fired to 1100oC in electric kiln.-
- White earthenware
- flowers
-
(and 2 more)
Tagged with:
-
From the album: 2016
Thrown bowls, cut at right angles to the rim. Thin slabs textured with bark, stamps, shells etc. - pieces attached to back part with front cut edge eased forwards to emphasise the contrast between the organic and engineered. Oxide washes applied at dry greenware stage, fixed in the bisqued firing. 3 back pieces were dipped in transparent glaze, front one dipped in tin white (to cover a repair that fired a different colour!). Fired to 1100oC in electric kiln.- 1 comment
-
- Earthenware