Jump to content

Search the Community

Showing results for tags 'stencil'.

  • Search By Tags

    Type tags separated by commas.
  • Search By Author

Content Type


Forums

  • Ceramic Arts Daily Forums
    • Forum FAQ & Terms of Use
    • Studio Operations and Making Work
    • Clay and Glaze Chemistry
    • Equipment Use and Repair
    • Business, Marketing, and Accounting
    • Educational Approaches and Resources
    • Aesthetic Approaches and Philosophy
    • Int'l Ceramic Artists Network (ICAN) Operations and Benefits
    • Ceramic Events of Interest
    • Community Marketplace – Buy/Sell/Trade/Free

Find results in...

Find results that contain...


Date Created

  • Start

    End


Last Updated

  • Start

    End


Filter by number of...

Joined

  • Start

    End


Group


AIM


MSN


Website URL


ICQ


Yahoo


Jabber


Skype


Location


Interests

Found 6 results

  1. I'm using 4 mil Mylar stencils. Glaze tends to crawl under the edge of the stencil which takes a lot of work cleaning up. I have tried making the glaze quite thick with CMC. This is helpful but it is not getting the job done. I am careful to brush away from the stencil. Suggestions please
  2. From the album: 2016

    Experimenting with bought tissue transfers and stencils as resist. Thrown white earthenware. Dipped in transparent glaze & fired to 1100oC in an electric kiln.
  3. From the album: 2016

    3 creamers with cobalt tissue transfers applied through a home made stencil with transparent glaze over. Wedding favours - 2 test pieces (120 in total) glazed with Mayco Stroke and Coat. Individual name tags to be attached using teal ribbon. These are for my niece (a labour of love) - would never be cost effective as a commercial item, unless someone had money to throw away! Fired to 1100oC in electric kiln.
  4. Celia UK

    Creamers

    From the album: Playing with mud 2016

    White earthenware. Underglaze and Japanese tissue transfers used over negative cut stencil. Waiting to be glazed.
  5. From the album: Playing with mud 2016

    Small white earthenware creamer decorated with Japanese tissue transfer over a negative transfer test I cut on my silhouette cutter. Not glazed yet. Blue and white with a modern twist.