Stained stoneware with Mason stain 6339 (royal blue) and threw it with regular gray stoneware. We'll see how it fires! -
I use Southern Ice porcelain, bisque fired then sanded then fired to cone 9 and sanded again, I don't use glazes. I have started making complex neriage coloured work, using the same clay body. I sometimes develop fine cracks that can successfully be patched and refired to cone 9 but the result is an all over tiny bloating of the surface. I have read a lot about bloating and the possibility it is due to over firing but don't really know what that means. I have twice fired thinner, slip cast work (from the same clay) without developing this problem. Could it mean I need to slow down the firing at one or more stages?