Thrown bowls, cut at right angles to the rim. Thin slabs textured with bark, stamps, shells etc. - pieces attached to back part with front cut edge eased forwards to emphasise the contrast between the organic and engineered. Oxide washes applied at dry greenware stage, fixed in the bisqued firing. 3 back pieces were dipped in transparent glaze, front one dipped in tin white (to cover a repair that fired a different colour!). Fired to 1100oC in electric kiln.- 1 comment
-