Hi all, I'm hoping someone can give some technical tips on repairing my Cromartie Hobbycraft kiln with controller and which is not hard wired but runs off a 13 amp plug. It is a top loader.
Bought as a used kiln, I have been using this quite happily for a number of years until recently where it has stopped reaching a stoneware glaze firing of 1240C.
I have replaced the elements and ceramic insulators, checked and cleaned up all the connections and tightened the belts around the body and lid. I have also changed the electrical lead from a short one which fitted into a socket not on the main circuit to a longer lead, about 5-6 meters, to reach a socket on the main circuit as I understand it can cope better with the energy required. I wondered if it makes a difference that the lead is much longer than the original which was no more than 2 meters.
Any advice or tips will be very gratefully received.
Thanks
Kathy