Jump to content

Search the Community

Showing results for tags 'bowls'.

  • Search By Tags

    Type tags separated by commas.
  • Search By Author

Content Type


Forums

  • Ceramic Arts Daily Forums
    • Forum FAQ & Terms of Use
    • Studio Operations and Making Work
    • Clay and Glaze Chemistry
    • Equipment Use and Repair
    • Business, Marketing, and Accounting
    • Educational Approaches and Resources
    • Aesthetic Approaches and Philosophy
    • Int'l Ceramic Artists Network (ICAN) Operations and Benefits
    • Ceramic Events of Interest
    • Community Marketplace – Buy/Sell/Trade/Free

Find results in...

Find results that contain...


Date Created

  • Start

    End


Last Updated

  • Start

    End


Filter by number of...

Joined

  • Start

    End


Group


AIM


MSN


Website URL


ICQ


Yahoo


Jabber


Skype


Location


Interests

Found 14 results

  1. I have been wandering from years ,talked with many pottery experts but haven't got anything closest to yohem tenmoku glaze recipe, So is there anyone who can help me out to figure it how these wonderful bowls are done .
  2. From the album: Bowls

    Fired to ^6, Bee mix 5, 4"x 7.5", rolled over rim, 3 Tiger sprigs, Glaze is Waterfal Brown from, Mastering ^6 glazes. 1.5#'s.
  3. From the album: Pottery 2016

    © Giselle No. 5 Ceramics, all rights reserved

  4. From the album: Mad About Pottery

    Nesting pottery bowls. made of speckled clay, I then coated the inner surface with a lovely rustic white glaze. b

    © Gittit Rad-El

  5. From the album: Work in Progress

    To date this is the most I've ever thrown in one session. A full half box of clay and ohhh were my hands ever sore the next day.

    © Copyright Giselle Massey 2015

  6. I don't even remember when someone advised me that flipping bowls so that the rim is on a flat surface, while drying, would reduce the amount of warping...but it is a practice that I still follow. I keep seeing studio images with drying shelves full of bowls, and the bowls are resting on their feet with the rims upright. OK...so, here are my questions: Is there any validity to the claim that drying bowls with the rim down reduces warping? Is there some point in the drying process where flipping bowls over evens-out the drying? Is the practice/preference more dependent on clay choice (i.
  7. From the album: Favorites

    Set of butterfly bowls I just finished. I'm fairly pleased with how they came out even though they were over fired.
  8. Hi All, I'm a high-schooler taking a Ceramics II course, and I love it! I specialize in wheel throwing and I'm really interested in fusing glass on ceramic pieces. How would I do this? My teacher recommended putting marbles in my bowls to melt the glass with the glaze, but I'm curious on what others have to say! Also, where can I either get special glass, or get marbles to melt! Write me back! Thanks, Travis
  9. Greetings! This will be my first time posting, so I hope this question is relevant. I was in the studio today doing some trimming. Trying to create a small foot, I ended up trimming too much and went through to the inside of the bowl. I tried to salvage it by bandaging it up with some more clay, hopefully it holds up. Is there any way to tell at what point to stop trimming (taking into consideration the weight of the bowl)? I really like the aesthetic of a small foot and the visual effect of the bowl looking like it's hovering. However, I end up trimming too much when trying to achieve th
  10. From the album: Translucent porcelain

    Translucent porcelain:wheel thrown,altered and carved. Interior glazed. Electric fired to cone 10. Southern Ice.
  11. From the album: Translucent porcelain

    Translucent porcelain:wheel thrown,altered and carved. Interior glazed. Electric fired to cone 10. Southern Ice.
  12. From the album: Translucent porcelain

    Translucent porcelain:wheel thrown,altered and carved. Interior glazed. Electric fired to cone 10. Southern Ice.
  13. From the album: Translucent porcelain

    Translucent porcelain:wheel thrown,altered and carved. Interior glazed. Electric fired to cone 10. Southern Ice.
×
×