From the album: Tornado Pot Sketches and Progress Images
I slipped this container into a tall spot in the kiln at the last minute to see how my glazes break over the undulating walls. Actually, I really needed the pot for the Anthurium that I received as a birthday gift back in January...it was quite root bound and begging for better living conditions.
Container is about 13" tall, stoneware, fired to cone 10 reduction and glazed with a combination of Ohio White, Woo's Blue, and Clear (sprayed on in overlapping layers).