Search the Community
Showing results for tags 'Glaze'.
-
Hi there, Like many artists, I am currently transitioning from making pottery in a community studio to working at home which is a big adjustment with an even bigger learning curve! I'll be setting up my very first kiln in the coming weeks and now need to figure out (for the first time) what the best commercial glazes out there are for the clay I'm using. For now I am using Standard #112 clay, and I will also eventually be working with their #551 Porcelain (both cone 6). I will be firing in a Skutt Km818 electric kiln. I have two big questions. First, does anyone have any tips
-
I am wondering if anyone has tried using the paint spray guns from harbor freight that run around $16.99. Or is it a you get what you pay for situation and worth the $50 to buy the PH300 glaze sprayer from the ceramic suppliers? Do paint sprayers even work for glaze, or will the just get all clogged up? I make 1" ceramic pendants and hand brush the fronts and backs. two coats on the back and three on the top. I currently have hundreds to do, and I think the time saved by using a spray gun will be the way to go.
-
Hi all, pretty new to the world of creating my own glazes - I have found several on glazy.org that I like (although I'm aware that an opensource online forum for glazes can be potentially disastrous). The question that I have is for silicon carbide. The recipe I'm referencing is this https://glazy.org/recipes/20474 which calls for a 1200 mesh SiC. The original recipe - https://glazy.org/recipes/19163 - calls for 1000 mesh SiC. The pottery supplier in my area carries only 400 mesh. What would the difference in appearance be? There's a massive difference in how those two glazes look and I w
-
Hello, I recently bought some OH10 (they were out of OH6) and was told I could just fire at cone 6 and everything would be fine. Then I was told the pieces wouldn’t vitrify and would be too porous for use (mugs and bowls). The studio will bisque the OH10 for me and asked if I have my own cone 10 glazes. The question is, can I fire my cone 6 glazes on the cone 10 bisqued pieces? Thank you for the help! Josh
-
Hey guys! I'm looking to make a sink basin for my bathroom in the upcoming months. I want to use Standard Ceramics 266 Dark Brown Clay with a turquoise/seafoam glaze on the interior while leaving the exterior bare. Attached is an idea of what I would like to do. I have never used a dark clay before, so I don't have experience to work off of and can't make test tiles until it is safe to use the studio again. Would coating the inside of the clay with a white underglaze cause the blue glaze to stand out more? Does anyone have a good glaze suggestion that stands out and reacts well to this clay? O
- 6 replies
-
- glaze
- underglaze
-
(and 1 more)
Tagged with:
-
I’m on a really long and frustrating journey trying to find a glaze/clay match to avoid crazing. But why, time and time again, on YouTube and Instagram am I finding potters with high follower numbers and ‘JUST SOLD OUT ETSY RESTOCK’ posts who are advertising pots, which have clearly got crazing issues?? Is there a ‘generally accepted’ level of crazing one should expect? Is it ‘normal’ to hear your pottery ping when getting it out of the kiln then later pouring hot liquid in? I’ve been driving myself nuts, but it appears to not be as serious as I initially thought... am I wa
-
Super newbie to the world of glazes. I have a few recipes from a trusted source, and upon recommendation I purchased several mason stains to add to a base glaze for an inexpensive and stable option. I used the super basic 20x5 base glossy glaze and added my stains to that as a trial. Some of them are great, but most of them are homogeneous in appearance. There's no variegation, it's not very interesting to look at. I'm wondering if there's something I can add to the 20x5 recipe, or a different clear glossy base glaze that would give the stains a more variegated appearance. Any help is apprecia
-
Hi all. Am having trouble with pinholes. I am using some commercial glazes and one glaze I mixed up from a recipe I found online. I clean my pieces very well before I glaze. I allow to dry before glazing, and leave them covered until glazing. I believe maybe it could be my one glaze recipe, or perhaps it could be the firing. I rent a space and the owner does the firings. He will not let anyone else fire and he blames all defects on you or your pots. Any help is so much appreciated. I am attaching a photo of a bad example of a glaze with a pinhole I got this firing.
-
From the album: Clay Tests
© TJA 2020
-
Hi there! I am wondering if someone could help me with converting this formula to use a different Feldspar. Possibly give me a good explanation as well.
-
Newbie here. I started in November and have fired my kiln four times (2 bisque, two glaze) with pleasing results. I use Amaco Stoneware Clay 38. Typically I fire it to cone 7 (I was shooting for cone 6, but my kiln fires hot). Recently I found this info connected to the clay I buy: "Bisque fire to Cone 04 (1971°F, 1077°C). The firing range is Cone 5–10 (2205°–2381°F), and the recommended glaze firing is Cone 10 (2381°F). At Cone 5 (2205°F), shrinkage is 13% and absorption is 7%. At Cone 10 (2381°F), shrinkage is 15%, absorption is 1.4%, and the clay fires white in oxidation and
-
Hi! I was running a cone 5 glaze with my skutt electric kiln and forgot to turn on my enviro vent. When I realized it was already finished and at 500F. I have the KMT so was able to see a graph of the firing which looked fine, but it did fire in 4 hrs instead of the regular 13hrs. What problems could this cause ??? Could this hurt my kiln for future firings? Vent is on now and another fan in the studio cause it definitely smells. Thanks!
-
Long time listener, first time caller here. I love the Turquoise Matte glaze from Coyote, but it isn't food safe. If I used a food safe glaze on the body of the mug could I still use the matte glaze on the handle or should I keep all glaze on the mug food safe?
-
I’m looking for a good stable cone 6 crawl for use with Mason stains. The crawls with Mag Carb and Nepheline Syenite tend to burn out some colours at cone 6. Thinking that some Frit 3124 substituted for some of the Feldspar might do it but any pointers would be appreciated.
-
I'm looking for some commercial glazes that show up nice and bright on Laguna's electric brown clay body.. light greens or blues, maybe even some pastel pinks or purples? Any suggestions? I've got enough options for darker, more natural looking glazes but want to expand to something lighter, brighter, cheerier...
- 6 replies
-
- electric brown
- glaze
-
(and 1 more)
Tagged with:
-
Hey I have tried to paint already glazed tiles with ceramic paint( it's paint for hobby ex.pebeo paint for ceramics and porcelain) and bake it in 250C. The result is ok but not secure for using these tiles on a bathroom or a kitchen ( the paint will faint after a while without glaze). Would you suggest me to use glazed paintings instead? What’s your experience with them?
-
Hey everybody! Brand new member but seasoned artist (to an extent). I have a very specific thought/question in mind that I cannot for the life of me find the answer to on google. I'm wanting to use some sort of high silica and/or high flux glaze to intentionally pool INSIDE the bottom of a bowl to make a sort of clear water effect. Would Shaner clear do just fine? or should I alter the recipe of some other clear glaze? Mix a whole new one? How thick can I make the glaze before it doesn't come out right? For best results should I pour it in layers or all at once? I fire at ^10 so high fire glaz
- 14 replies
-
So, I've been working on two slab projects for the last 2 weeks. Both of them have some pieces in the 3rd dimension as well as lots of 2D detail. I finished constructing both pieces today and despite how shaky my hands were, managed to paint both almost immaculately. Thing is, I forgot to give them a bisque firing before I jumped into glazing them. They're so detailed that there's no way I can remove the glaze without destroying the work in the process, so unless there's another way to make finished work out of them, they're garbage and I wasted my time, materials, and effort. My instructo
-
Hello! I’ve heard that you can fire greenware with glaze up to cone 6 in one go- ive never done it myself though. Is this something that actually safe for the pottery? Do I need to do it in a specific way? Fire in a specific way? Any input would be much appreciated!
-
Hi ! I am so glad I found this forum. I am trying to kick start a ceramic club. Here at our facility we have our Kiln room that is fully equipped, completed with endless amount of supplies. I really hit the mother load, however this room has not been utilized in ten(10) years or so. We have EVERYTHING, but nothing has an expiration date. I've been into ceramics since high school, unfortunately this is just something I am not familiar with. Most of our supplies are either Mayco or Duncan Bisque, I might call customer service to check with them about their under glazes, glazes, paints and such.
- 2 replies
-
- kiln
- earthenware
-
(and 4 more)
Tagged with:
-
I fired a sculpture using 2 coats of low fire O with one coat of A on top. The results where muddy. I would like to refire it. It turned out brown when it should have had more turquoise. What would happen if I put a thick coat of O 66 on top?
- 13 replies
-
- glaze
- layering glazes
-
(and 1 more)
Tagged with:
-
Hi, I am a VERY amateur artist but I like to experiment with clay and sculpting. I recently used Sculpey oven-bake clay to create a bowl (flat at the bottom, more like a mug without handles haha). I applied 2 coats of Sculpey gloss glaze all over. It was pretty successful so I’m now inspired to make some mini teacups! My bowl is waterproof due to the glaze, but would hot water ruin the teacups/glaze in any way? Thank you so much!