  1. I recently got a older Cress C-11-H and I don't know anything about it.

    I was informed that it did not get up to temperature, but that is all I know. It did not come with a manual. I tried watching some videos on how all the parts are supposed to look and I think my kiln sitter needs to be replaced, since the kiln piece that holds it is worn through. 

    I can't seem to find any of the parts that I need. Is this kiln to old to find replacement parts? I don't know how to tell the age.

    I don't know that the kiln sitter would cause it too not reach temperature. Does anyone know how I can fix that? Do I need to get new elements?