Thank you Diesel...I have found several different recipes with various formulations. Some by weight, parts, percentage, and one that was listed as proportions. As a newbie it was a little confusing, but the one listed on The Claybucket site seemed reasonable, especially if a college is using the recipe as their primary clay and all components were readily available at my local ceramics shop. I just did not want to mess it up and figured I would ask some folks who have been doing it for a while.
-
Thank both of you for responding - looking to make highfire claybody. I full understand the accuracy of weight over volume, but with the recipe as listed it would be a wildly different formula on weight versus volume, that is why I questioned it. I was just not sure when I see recipes listed as "parts" if it was weight or volume in general unless otherwise specified. Again - thanks for the responses. New to the art and trying to learn.
-
New to pottery and currently exploring clay recipes. I found a stoneware recipe "IUS Shop Stoneware" and the recipe is in parts. Probably a silly question, but I am new and do not understand if these parts are by volume or weight. Can anyone explain how clay recipes in "Parts" are actually measured out?
Clay Recipe in Parts? Weight or Volume?
in Clay and Glaze Chemistry
Posted
That makes sense, thank you.