  1. Mine has a cap on it I think? I’m inwardly very new to the thermocouple and electronic controller thing so I don’t know what im looking at.
  2. Hi all, first time posting. I recently aquired and olympic 1818HE with a Bartlett rtc1000 controller on it. I know the controller is made more for glass or heat treating kilns but have seen it used for ceramics without problem. I had a few error codes in my first two firings, the first was e3 during my final hold at cone 04. The code chart states that the temp fell 50* below final hold temp during the hold and the chart says that’s a relay failure. I did a full power test at r9999 to f1000 and all of the elements glowed a beautiful red. I assumed that beca
×
×