  1. This sounds exactly like what happened... the gas just didn't have enough oomph to get up over 2300. Thank you Mark!
  2. Hello potters! After running a Skutt electric kiln for years -we moved to a mountain retreat at 5300 feet and switched to a brand new propane powered Olympic 2831g gas kiln. After running a few bisque firings to cone 04 - we had zero issues. Ran a glaze firing Friday night - cone 10 reduction - started at 10:30pm - topped out at 2283 degrees - could not would not budge beyond that - added gas - lowered the gas - increased air flow - decreased air flow tried closing the damper - opening all the way - literally every tweak we could think of - nada.... wouldn't go any higher and a
×
×