  1. The specific gravity is 1.96 I added water to get it to 1.75. will see what that does first. How do I counteract the darvon 7 if we added to much? Thanks
  2. Had slip in pouring table to long and slip hardened. It is low fire slip. We added water and add casting slip thinner. The slip seems thin enough but parts of greenware are collapsing while drying in mold. It was not emptied to quickly. It has desired thickness, but a portion of the greenwear collapses. It stays soft. It also seems to thicken up and not drain well. Any help is appreciated. Paul
×
×