  1. Min- I am a little confused by your post. You note that my recipe does not have any manganese. You suggest adding manganese to my it. It is already 70% manganese.
  2. I am looking for a recipe for a ^5-^6 glaze (oxidation) that mimics rust. I have attached an example of what I am looking for. The glaze attached was fired at ^8-^9 oxidation. 5-6 second dip Viscosity of whole milk Manganese dioxide 70China Clay 23Copper Oxide 7 I tested it at ^5 but it ranged from bronze to black depending on the glaze thickness. As I mentioned I need something that will work at ^6. Any ideas?
×
×