ı have a simple press and a mold for porcelain handle. Unfortunately, the clay which ı prepared doesnt work well . when ı put the clay into mold and press it the last product comes with little fractures. To prepare the clay ım using oil for it and using a mixing machine. ı need an appropriate recipe for clay. if you have other ideas to make it better please enligthen me .