Jump to content

Kilnnewbie

Members
  • Content Count

    3
  • Joined

  • Last visited

  1. Hi- Any thoughts on use of stilts vs cookies for firing 06-04 glazed earthenware ? Have seen both recommended. Cookies seem a bit easier as no grinding off points, but stilts seem recommended much more often. This is my first kiln, so not sure which direction to go. As I am new at kiln work, don't want to ruin any shelves! THanks for any input. Barbara
  2. I am a bit late to this post. I like the idea of cookies more than stilts and cutting off stilt marks. However, I am firing low fire, usually 06-04 in my first kiln. Most info I see recommends stilts. Any thoughts? Thanks for any suggestions!
×
×