  1. My husband was another pair of hands. Gently turned it onto a styrofoam ring.
  2. Thanks, but it woldn’t share. I have bad luck with this stuff. I managed to figure it out though, so the clay is okay.
  3. I can’t reduce the file size from my phone to send a photo.
  4. I made a 14” porcelain platter and cut many negative spaces into it, about 1/4” thick. It is loose on a plaster hump mold. I can’t flip it with the mold as it will crush the clay. I forget to put tabs under it. Anyone have any ideas to get it off?
×
×