Hi Mihai,
Just wanted to check how you're getting on with this project? I'm planning to build an efficient ceramics kiln for my partner that's pretty similar to yours. My planned specs are: 30cm x 30cm x 40cm, front loader, made from 50mm ceramic fibre board, backed up with 75mm ceramic fibre blanket, and with an aluminium case. We have 16 amp circuits too, so I'm looking to power the kiln at about 3000 watts / 13 amps. Aiming to get it to around 1280 degrees C. I'm shopping around for some 1.8mm Kanthal, looks quite expensive. I bought a ramp / soak PID controller from AliExpress, hopefully that works fine.
Would be very keen to hear about your progress!
Cheers
Ollie