  1. No that is the picture from the amaco brochure. Showing how the glazes are layered. The finished product was suppose to be more blue. My results were muddy. I think the orange glaze was too thick. Wondering if I put the opalescent glaze on top of it and refire will it look more like the picture? So layers would be O over AC over O.
  2. This is what it was supposed to look like. Instead it’s muddy brown. I have had success with this technique before and with other pieces in the firing.
  3. I fired a sculpture using 2 coats of low fire O with one coat of A on top. The results where muddy. I would like to refire it. It turned out brown when it should have had more turquoise. What would happen if I put a thick coat of O 66 on top?
×
×