  1. Thanks everyone! I have now compiled several clear gloss and clear satin matte recipes. With John Britt's book on order, I think I have a good start to work with! Luckily I am a member of a potter's studio so I don't have to buy small amounts of all the ingredients. Lot's to do!
  2. Thanks but yikes! The first book sells for 179 bucks! ok, just priced the other one, that I can afford! Thanks!
  3. Does anyone have a simple clear gloss recipe that you love for cone 6 ox suitable for clear and color? Simple, stable and preferably cheap. Same for matte surface. Prefer a soft satin matte, not too dry. Thanks!
×
×