  1. Thanks for your responses. I think what you all said is pretty much what I expected. I know the pitting isn't really a problem, just thought the coating might prevent the aluminum from reacting with porcelaneous clays. I certainly don't want paint bits in my clay! I think I'll just leave it alone!
  2. I have been using an aluminum barreled Bluebird pug mill for many years. I understand that the aluminum can have a chemical reaction to porcelaneous clays, also, the barrel has become pitted. I am considering having the barrel powder-coated to solve both of these issues. Does anyone have experience with powder-coating aluminum pug mill barrels? Are there potential problems I should be aware of? My biggest concern is the possibility of coating material wearing off and contaminating the clay.
×
×