  1. hello I trying to use De air pugmill to eliminate the air bubbles in my clay, that mixed from 2 local clays. After 3 times pugging, it still inside the clay when it throw it on wheel. but i 've checked by cutting into thin sheet thickness around 5mm. , there is no air bubbles there. Anyone have faced this problem, and how to solve it because now we have quite a lot stock for this clay. Ps. I did some solutions like - pug more 3,6,9 times -wedge more 300,600,1200 times/5kg. - add some addition beer, vinegar - let it dry 3-5days but it'
×
×