Throwing wise- I like to throw a thick cylinder, push it out and then color in the next. For lamps I prefer to have the top part of the belly be a little flatter. (usually fits the shape of the shade better.)
Glazing, a crystalline glaze, 6 copper oxide with 1 gram of ilmenite.
I think I fitted this with gold hardware.
-
That is awesome!
-
*This is a lamp stand if you are wondering why there is such an unorthodox neck*
-
10 hours ago, glazenerd said:
Predicting color break in relation to anticipated glaze run is a science of its own.
Only had two in this load that came out well. I'm definitely getting better at it. This was 1/3 white and 2/3 green.
-
On 12/23/2019 at 7:19 PM, Mark (Marko) Madrazo said:
Nice work. I have plans to do this. Thanks for sharing.
It's not as hard as people say, just do a lot of reading and learning before you try!
-
On 12/24/2019 at 9:55 PM, Denice said:
They remind me of lily pads floating around in a pond. Denice
Don't they! Thats what I always thought of with this glaze.
April 2020 vs October 2019 Progress!
in Browse Member Galleries
1Posted
April 2020 vs October 2019