  1. Hi, so I am new at this and asking for help. I had fired my clay, and painted it (with regular paint, ceramics friendly) and then put a glaze over top. The glaze said it could be used over paint and that it should be clear after firing. After firing the glazed pieces, it seems that the paint has been stripped off and the glaze never went clear. Did I do something wrong? My kiln is a cone 8, bought barely used. I followed the instructions on the side and the internet: Cook on low for 1 hr., medium for 2 hrs., and (after looking it up) another hour on low. Also, is there any way I can fix the pieces? They were gifts and took me a while to make them, but I know they're likely ruined. I appreciate any advice and help.
×
×