  1. Hi I am new to clay and throwing and starting out I got Amac oA-11 mix white stoneware clay and while I know I am still learning this clay seems extremely finicky in terms of water and how fast I throw ( beginner, so think more water and slower) . I threw a bowl the other day with a porcelain clay by New Mexico Clay and no problems at all, went home tried the exact same thing that I did in class, clay everywhere! has anyone used this clay ( Amaco) andany issues you found with it? Thanks for your help
×
×