Not sure about this one specifically, but google Magda Gluszek and I see similarities. Animalistic impulses with human consumption and social behavior. Here is an article https://ceramicartsnetwork.org/daily/ceramic-art-and-artists/ceramic-sculpture/from-maquette-to-form-creating-figurative-ceramic-sculptures-from-a-clay-sketch/
-
5a99f54ebebd7_floridaleafpotsbowls006.JPG
Kathy P commented on oldlady's gallery image in Browse Member Galleries
-
Beads Pendants Cabs Minis Low Fire Ceramics
Kathy P added images to a gallery album in Browse Member Galleries
Standard White 105 low fire cone 05 Paragon SC2 kiln - Feb 20, 2018 very first bisque firing of very first pieces. -
From the album: Beads Pendants Cabs Minis Low Fire Ceramics
Those squiggles on the bird chin! -
Kiln shelf planning before loading for glaze firing
Kathy P posted a gallery image in Browse Member Galleries
From the album: Beads Pendants Cabs Minis Low Fire Ceramics
Planning the setup before loading the kiln. -
From the album: Beads Pendants Cabs Minis Low Fire Ceramics
Bead rack tree tower with high temp wire. Clay pattie (tortilla thick, unfired) under glazed cat. High temp wire embedded in clay pattie as a stilt. This is my first glaze fire. Can't wait to see the kiln open! -
From the album: Beads Pendants Cabs Minis Low Fire Ceramics
I used Liquid Bandaid as a resist on the bird so I could scratch in lines and fill with black. -
From the album: Beads Pendants Cabs Minis Low Fire Ceramics
Glazing tiny details, preplanning the steps like a recipe. First 2 ever ceramic pieces glazed and I'm already experimenting. I used Liquid Bandaid as a resist on the bird so I could scratch in lines and fill with black. -
From the album: Beads Pendants Cabs Minis Low Fire Ceramics
Very first batch of low fire clay pieces. All loaded onto a 5X5 inch kiln shelf. I have a Paragon SC2 kiln that I named Miss Piggy. I use it often to anneal steel rods for making stamps and I fire metal clay silver and bronze. This first bisque firing was thrilling! 15 hours, very conservative ramp rate. Like the first time trying to dress a newborn, I was being super careful.© yorkavenuestudio.com
-
From the album: Beads Pendants Cabs Minis Low Fire Ceramics
Very first batch of low fire clay pieces. All loaded onto a 5X5 inch kiln shelf. I have a Paragon SC2 kiln that I named Miss Piggy. I use it often to anneal steel rods for making stamps and I fire metal clay silver and bronze. This first bisque firing was thrilling! 15 hours, very conservative ramp rate. Like the first time trying to dress a newborn, I was being super careful.© yorkavenuestudio.com
-
Clay dries too fast in hands, dry skin?
Kathy P replied to Kathy P's topic in Studio Operations and Making Work
hateful clay, haha, right?!? Is there a place on the forum to just blab when something exciting happens and I just want to tell someone who would understand? Like finally finding a place that offers kiln sharing! Or successful firings photos? I want to follow the rules -
Clay dries too fast in hands, dry skin?
Kathy P replied to Kathy P's topic in Studio Operations and Making Work
Will do! Damp box, research new clay (talc content) and damp work surface. Thank you! I have Gloves in a Bottle that I use when working with metal clays. Would lotion on my hands end up with compromised clay and separation issues? I might try a bit as a test. Also will try Paper clay slip recipe and see how that feels. Most annoying cracks are when bending a snake roll. -
Clay dries too fast in hands, dry skin?
Kathy P replied to Kathy P's topic in Studio Operations and Making Work
Main floor in home, and not noticeably dry. Room temp a little cool. I’m curious if others have come across this, where a persons skin chemistry or ? makes clay dry lightning quick. I see demos of handbuilding where the clay is dreamy perfect for long time and rarely fingerprints. I get either sticky or dry with almost zero dreamy, haha. -
Help needed: The clay I'm forming by hand gets cracky and splits so fast that even a simple form isn't finished unless I'm rushing. Please suggest ideas for longer, less rushed forming time. I'm using low fire clay, Standard White 105 brand new from the box and pinching and forming animals and small pendants and beads. I can roll out a snake and then it's too dry. That fast. I can roll a bead and pinch a couple times, then cracks start if I continue. Super dry hands maybe? My guess is to use a mist spray, cover, wait, work a few minutes, mist, cover, wait...