  1. Hi all, i'm using clay slurry + 40% RIO
  2. Hi, i'm having trouble with iron oxide slip applied at the greenware stage. i've noticed that a thin layer gives varied colours and a thick layer gives either black or nothing- does it burn off? (i use a transparent glaze over this) additionally, a lot of the colour washes out on cleaning after bisque. what's going wrong and how can i stablize the slip to give me a solid black? i use stoneware fired to cone 09 bisque and cone 6 glaze. thanks!
×
×