  1. Matt Oz

    some work

  2. From the album: some work

    Night light made with translucent porcelain I've been developing that fires almost to a glass. Fired items come out of the kiln with an appearance similar to fused glass, no glaze necessary. Because of slumping the clay works best with flat items or ones supported during firing.
  3. From the album: some work

    Slab and press mold construction. Translucent porcelain
  4. Thank you, I'm glad they look yummy, I only use pure can sugar in the recipe.
  5. From the album: some work

    Plates made from a cone 6 porcelain I've been developing that fires almost to a glass, has to be fired flat or in a mold. colored with Mason stains.
  6. Matt Oz

    Tree lamp day

    Thank you Frederik. I had a photo of a lit lamp, but it wasn't very good, so I posted a new one that's a bit better. One of these days I'm going to have to buy a newer camera.
  7. From the album: some work

    Slab and press mold construction. Translucent porcelain lamp shade.
  8. From the album: some work

    Slab and press mold construction. Translucent porcelain lampshade
  9. Offcenter, I agree, it is difficult to show. I thought your video worked well, movement seems to help. I have not yet used Frost or Ice, but I have done many tests using the same New Zealand kaolin, and as far as I can tell using this clay body with NZ kaolin should be more translucent than them, but only because this clay is so highly fluxed and has lower clay content. It has to be fired in a form, or on something flat, and is actually glassy when mature. Thanks for your question. And thanks Trina
  10. From the album: some work

    Test Plate using experimental porcelain
  11. From the album: some work

    Porcelain hand sculpture
  12. Matt Oz

    Leaf lamp

    From the album: some work

    Leaf lamp with porcelain lampshade
×
×