  1. Rakuken

    image

    From the album: Ken Kang

    23 inches height. Copper red, applied ash glaze. Cone 10 reduction fired.
  2. Rakuken

    Vase

    From the album: Ken Kang

    ht. 12 inches. Gas fired cone 10 reduction. Applied ash glaze, (Kingsford briquette BBQ ash)
  3. Rakuken

    Sake set

    From the album: Ken Kang

    Gas fired, cone 10 reduction
  4. Rakuken

    Sake set

    From the album: Ken Kang

    Cone 10 stoneware, gas kiln Shino glaze
  5. Rakuken

    Pahoehoe

    From the album: Sculpture

    Stretch and rolled with wood dowel inside. Applied ash glaze, fired upside down, cone 10 reduction. 20 inches across at the top. Welded bronze stand.
  6. From the album: Ken Kang

    Wheel thrown, 7 in. ht., fired on it's side on clam shells, applied ash glaze, gas fired to cone 10. I shape and finish all my wood covers. Bamboo addition
  7. From the album: Ken Kang

    Wheel thrown, altered, 3 inches ht., Chinese crackle glaze, cone 10 Turned wood cover, refinished black and red
  8. From the album: Ken Kang

    Hand built, 8 inches ht., applied ash glaze, cone 10 reduction I shape and finish all my covers. Bamboo handle
  9. From the album: Ken Kang

    Wheel thrown, altered. 2 1/2 inch ht. Copper red glaze, cone 10 I shape and finish all my wood covers.
  10. From the album: Ken Kang

    Hand built, 8 inches ht. Copper red glaze, fired to cone 10 I shape and finish all my wood covers. Bamboo handle
  11. From the album: Ken Kang

    Hand built, 7 inches ht., applied ash glaze, fired to cone 10 I make and finish all my wood covers. Bamboo handle
  12. From the album: Ken Kang

    Thrown, Copper Red with Nuka glaze. Cone 10 reduction
  13. From the album: Ken Kang

    Thrown, applied ash glaze, cone 10 reduction Fired on it's side on clam shells.
  14. From the album: Ken Kang

    Electric kiln converted to propane. Two forced air burners. Firing to cone 10 Two collars, removable for loading wares.
  15. Experimented with glass beads in wet clay. It's safer than using shards from bottles etc. Using the beads for necklaces, many colors and shapes. Aloha, Ken
  16. From the album: Ken Kang

    13 inches tall. Wheel thrown, altered Applied ash glaze, fired to cone 10
  17. Rakuken

    ash glaze

    Kingsford Briquette ash, unwashed, no additives, cone 10. height: 23 inches