  1. I have a glaze that has been formulated and mixed properly in the past. This time however I cannot stir; it settles on bottom of bucket, I have added the correct amount of bentonite as recipe calls. It is a recipe that calls for crocus martis stain. Could it be that the materials in the crocus martis has changed? Should I add an additional amount of bentonite? What is your suggestion?
×
×