  1. Thank you so much, John! I'll give it a try. Pam
  2. I have a recipe that is from a Walter Ostrom workshop. The glaze is called ^04 Moon. The ingredients don't add up to 100, and I'm wondering if I should go ahead and test it as written. Just thought I would see if anyone had any comments or suggestions. Thanks, Pam Mag carb 25 EPK 10 Lithium carb 5 Borax 20 Gerstley borate 10
×
×