  1. Hi I'm wondering if anybody has a recipe for a cone 10 reduction copper red glaze (I'm talking oxblood or peach bloom, NOT flambé) that flashes electric blue? I hear that if you use a feldspar based glaze and use a feldspar that is high in potassium and low in sodium (usually its the other way around) that the glaze will tend to have these blue flashes more. If you know a good recipe and have tried it yourself what cone does it work best around? I know that these glazes don't do best at cone 10 but rather around 8-9, but I still wanna hear your experience. Also, I like to do a quick oxid
×
×