  1. Hi there, I have been using Laguna 65 for years now and have enjoyed throwing with it and love the color once fired. I have been having serious issues with crazing from the beginning, and now with my new surface designs I would really prefer a good glaze fit. I have tried several different clears on this clay body including commercial Amaco HF-9 and several clears that I mixed on my own. ALL OF THEM have crazing. Normally delayed crazing. Of course this indicates that there is a poor fit with the glaze. But after all of the glazes I have tested I am wondering if there is something I am missing with the clay body itself? I fire to cone 6. I was wondering if anyone else uses 65 and has either A)found a clear glaze that works successfully for them or has suggestions for what I might be able to do to solve my issue.
×
×