Long dried pieces exploding in bisque
Kellykopp replied to smesa's topic in Clay and Glaze Chemistry
You can also try a "candling" program. I run the kiln at 180 degrees for 8 hours. Do not go above 212 degrees (boiling temperature), and be aware of any offsets your kiln may have. Make sure your work is not too thick. Sometimes I touch the piece to my face and if it feels cool I let it sit for a while longer. It's humid now in Indiana, I can't imagine what you go through in Florida! -
Ferric Chloride; Dilute or Not?
Kellykopp replied to ThruTraffic's topic in Clay and Glaze Chemistry
What Babs said, exercise extreme caution Ferric Chloride fumes are very toxic. -
We always had "Clay Gods" or "Kiln Gods" tucked into corners, on shelves, near kilns, etc. when I was at Herron. To continue the tradition, I have one in my studio sitting on a shelf overlooking a space where I work, as well as the kilns. When I look at her it brings back fond memories. Pres, those peep hole creatures are very neat....like them!!
-
John Baymore - Thayer Gallery Solo Exhibition - Feb. 2017
Kellykopp commented on a gallery image in Browse Member Galleries
- 2 comments
-
- John Baymore
- Exhibition
- (and 8 more)
-
Nesting Bowl Set in Teal and Chocolate Brown with Slip Trailing.
Kellykopp commented on GiselleNo5's gallery image in Browse Member Galleries
- 2 comments
-
- slip trailing
- red clay
-
(and 1 more)
Tagged with:
-
Modern style Bracelet and Necklace Set
Kellykopp commented on Pugaboo's gallery image in Browse Member Galleries
-
From the album: After 30 years.........
-
After 30 years.........
Images added to a gallery album owned by Kellykopp in Browse Member Galleries
A sampling of the last few months of barrel firing after being away from my beloved clay for 30 years..... -
From the album: After 30 years.........
-
From the album: After 30 years.........
-
From the album: After 30 years.........
-
From the album: After 30 years.........
-
From the album: After 30 years.........
-
From the album: After 30 years.........
-
From the album: After 30 years.........
-
From the album: After 30 years.........
-
From the album: After 30 years.........
-
From the album: After 30 years.........
-
From the album: After 30 years.........
-
From the album: After 30 years.........
-
From the album: After 30 years.........