  1. All of my forms are made with either Georgie's G-mix 6 or Georgie's Trillium Porcelain.  Image is carved into a layer of black-brown underglaze.  After the bisque I typically stain the decorated area with a dark glaze.  I'm experimenting with clear glaze thickness, some pieces have glaze barely brushed on while others have several layers of glaze. I use commercial glazes.

×
×