  1. Yes it is cone 6, I think I'm going to try more stains. I did try mason gun metal but it went very blue with all the base glazes I've tried. I have tried nickel and many different combinations with cobalt but no luck. I even thought about colouring the clay but most research suggests manganese which I don't really want to use. So I will see how colouring a slip goes but I don't think there is such a thing as a transparent satin matte. The search continues, thanks for the advice
  2. Hi, I have been testing for quite some to trying to get a light grey glaze with white speckles. Can anyone make any suggestions for a satin Matt grey glaze. For the white speckle I was planning on trying molochite but any suggestions would be greatly appreciated.thanks Jo
×
×