  1. Thank you very much. I'll try that. John
  2. I am trying to make a yellow underglaze for a white stoneware miller clay body. I fire a slight reduction to cone ten with a clear 'limestone clear' glaze. So far I have tried several mason stains including ms 6450 at twenty percent. Also I have tried titanium dioxode at fifteen percent. The mason stains are firing very clear and the titanium is not quite a yellow. I would love any suggestions. Thank you John
×
×