  1. Milk-firing Updated

    Experimenting with the Ukrainian method of washing a fired pot in milk, then bringing it to about 600°F and holding it there until the desired color is reached.

    This bowl was thrown from Runyan K-4 Multi-Purpose Red Brown Body, and fired to cone 04 prior to milk treatment. Following the milk fire, it was treated with a generous coating of beeswax and olive oil (2 parts wax, 1 part oil melted together) then heated to 200°F to allow the wax to soak in. Heating it released all the little bits of terry towel fluff that got caught in the wax upon application, and they just brushed off with a light buffing.
    Stellaria
    Album created by by
    Stellaria Updated
    • 4
    • 0
    • 1
    • 4 images
    • 0 comments
    • 1 image comment
  2. Spring Session '14 Updated

    Stuff made during my third Clay Club session - March to June 2014
    Stellaria
    Album created by by
    Stellaria Updated
    • 6
    • 0
    • 0
    • 6 images
    • 0 comments
    • 0 image comments
  3. Stamps Updated

    Stellaria
    Album created by by
    Stellaria Updated
    • 4
    • 0
    • 0
    • 4 images
    • 0 comments
    • 0 image comments
  4. Session 2 Updated

    Work from my second session of "classes" that are really just clay club work days and not actually instructional classes.
    Stellaria
    Album created by by
    Stellaria Updated
    • 9
    • 0
    • 1
    • 9 images
    • 0 comments
    • 1 image comment
×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.