  1. Thanks, it means a lot to hear from someone with more experience/knowledge.

  2. Hello, As Im moving from sculpting stone into porcelain, I have a million questions (even after reading extensively books & watching videos.) In particular, to figurine building but anyone working with porcelain could help. How long after taking a small piece out of the mold (slip casting) can other small parts be attached/glued with slip to the other piece? As I did not fire yet, will the parts hold together in the kiln? And is it reasonable to think that, if I made a figurine out of porcelain clay (hand-modeled this time) and fire the parts (arms, head etc) separately could they be glued (epoxy?) together? Thanks!
  3. my first self drying clay modelling work
×
×