  1. i am doing a sculpture larger then my kiln size. I need to cut it into sections in order to fire it. I do hand built sculptures. What I need to know is when I cut it apart to hollow it out do I need to place the sections back together so that they dry at the same rates. If i fire it in sections will it warp not being together in the kiln? Have to do in sections because lost the first one after 50 hours because to large to carry to the kiln because of composition of subject and can not place against body to carry. Any help? Have to finish sculpting it by Friday?
×
×