Jump to content

JohnnyK

Members
  • Content Count

    725
  • Joined

  • Last visited

2 Followers

About JohnnyK

  • Rank
    Advanced member

Profile Information

  • Location
    Citrus Heights, CA
  • Interests
    Ceramics, glazing techniques, photography, farming, reading all kinds of stuff but primarily thrillers

Recent Profile Visitors

11,353 profile views

Single Status Update

See all updates by JohnnyK

  1. Started to glaze the bowls but got an order for a dozen medium, tri-tube bud vases too...the first job for the extruder...

    1. Show previous comments  1 more
    2. glazenerd

      glazenerd

      Pics please when you finish. 

    3. JohnnyK

      JohnnyK

      Pix of the latest glaze run...the customer bought 13 instead of 10 bowls. 18-54,55 2nd is the same glaze pattern after removal of a defect in each bowl and firing again. All are Amaco PC glazes layered for effects. In some cases Duncan's RG704 Shino Cream was banded to create the white edge runs...

      18-50,51.jpg

      18-52,53.jpg

      18-54,55-2nd firing.jpg

      18-66,67.jpg

      18-68,69.jpg

    4. glazenerd

      glazenerd

      Clever use of glaze: creates visual interest. Well done!

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.